본문 바로가기 주메뉴 바로가기

Cobalt

home > 재료소개(Powder/Wire) > Powder-MCrAIY >Cobalt

Superior powders for superior coatings

Composed of nickel (Ni) or cobalt (Co) or a combination of both, MCrAlY powders are the foundation of gas turbine hot section thermal spray coatings. To create them, we use the industry’s most advanced Vacuum Induction Melting / Argon Gas Atomization (VIM/AGA) technology. The result is high-purity, low-oxide original equipment manufacturer (OEM) approved powders that produce superior high-temperature oxidation- and corrosion-resistant coatings. See our Co- and Ni-based MCrAIY powders below.

Powder Name&Composition Chemistry & Size DIAMETER Safety Data Sheet (SDS)
CO-242

Co MCrAlY

(Atomized)
Proprietary
  • Product data available through OEM
CO-242 (128KB)
CO-242-3

Co MCrAlY

(Atomized)
Proprietary
  • Product data available through OEM
CO-242-3 (128KB)
CO-249

Co MCrAlY

(Atomized)
Proprietary
  • Product data available through OEM
CO-249 (128KB)
CO-249-2

Co MCrAlY

(Atomized)
Proprietary
  • Product data available through OEM
CO-249-2 (128KB)
CO-249-4

Co MCrAlY

(Atomized)
Proprietary
  • Product data available through OEM
CO-249-4 (128KB)
CO-249-6

Co MCrAlY

(Atomized)
Proprietary
  • Product data available through OEM
CO-249-6 (128KB)
CO-249-8

Co MCrAlY

(Atomized)
Proprietary
  • Product data available through OEM
CO-249-8 (128KB)
CO-260-1

Co MCrAlY

(Atomized)
Proprietary
  • Product data available through OEM
CO-260-1 (137KB)
CO-260-12

Co MCrAlY

(Atomized)
Proprietary
  • Product data available through OEM
CO-260-12 (137KB)
CO-301

Co MCrAlY

(Atomized)
Proprietary
  • Product data available through OEM
CO-301 (131KB)
CO-301-3

Co MCrAlY

(Atomized)
Proprietary
  • Product data available through OEM
CO-301-3 (131KB)
CO-127

CoNiCrAlY

(Atomized)
Ni 32.0

Cr 21.0

Al 8.0

Y 0.5

Co balance

-45 µm/+5 µm
  • Excellent corrosion and oxidation properties up to 1900°F / 1038°C
  • Heat treating is required for optimum performance
  • Typically used for either a Thermal Barrier Coating (TBC) bondcoat or an environmental protection coating
  • GT-20
CO-127 (128KB)
CO-159

CoNiCrAlY

(Atomized)
Ni 32.0

Cr 21.0

Al 8.0

Y 0.5

Co balance

-75 µm/+16 µm
  • Excellent corrosion and oxidation properties up to 1900°F / 1038°C
  • Heat treating required for optimum performance
  • Typically used for either a TBC bondcoat or an environmental protection coating
  • GT-20
CO-159 (128KB)
CO-210-1

CoNiCrAlY

(Atomized)
Ni 32.0

Cr 21.0

Al 8.0

Y 0.5

Co balance

-45 µm/+11 µm
  • Excellent corrosion and oxidation properties up to 1900°F / 1038°C
  • Heat treating required for optimum performance
  • Typically used for either a TBC bondcoat or an environmental protection coating
  • GT-20
CO-159 (135KB)
CO-241

CoNiCrAlY

(Atomized)
Ni 32.0

Cr 21.0

Al 8.0

Y 0.5

Co balance

-45 µm
  • Excellent corrosion and oxidation properties up to 1900°F / 1038°C
  • Heat treating required for optimum performance
  • Typically used for either a TBC bondcoat or an environmental protection coating
  • GT-20
CO-241 (128KB)
CO-210-24 / CO-241-3

CoNiCrAlY

(Atomized)
Ni 32.0

Cr 21.0

Al 8.0

Y 0.5

Co balance

-45 µm/+16 µm
  • Excellent corrosion and oxidation properties up to 1900°F / 1038°C
  • Heat treating required for optimum performance
  • Typically used for either a TBC bondcoat or an environmental protection coating
  • GT-20
CO-210-24 (135KB)
CO-211

CoNiCrAlY

(Atomized)
Ni 32.0

Cr 21.0

Al 8.0

Y 0.5

Co balance

-90 µm/+38 µm
  • Excellent corrosion and oxidation properties up to 1900°F / 1038°C
  • Heat treating required for optimum performance
  • Typically used for either a TBC bondcoat or an environmental protection coating
  • GT-20
CO-211 (127KB)
CO-211-1

CoNiCrAlY

(Atomized)
Ni 32.0

Cr 21.0

Al 8.0

Y 0.5

Co balance

-38 µm/+5 µm
  • Excellent corrosion and oxidation properties up to 1900°F / 1038°C
  • Heat treating required for optimum performance
  • Typically used for either a TBC bondcoat or an environmental protection coating
  • GT-20
CO-211-1 (127KB)
CO-211-3

CoNiCrAlY

(Atomized)
Ni 32.0

Cr 21.0

Al 8.0

Y 0.5

Co balance

-150 µm/+63 µm
  • Excellent corrosion and oxidation properties up to 1900°F / 1038°C
  • Heat treating required for optimum performance
  • Typically used for either a TBC bondcoat or an environmental protection coating
  • GT-20
CO-211-3 (1270KB)
CO-110

CoCrAlY

(Atomized)
Cr 23.0

Al 13.0

Y 0.65

Co balance

-45 µm/+5 µm
  • Atomized, CoCrAlY alloy
CO-110 (128KB)
CO-110-1

CoCrAlY

(Atomized)
Cr 23.0

Al 13.0

Y 0.65

Co balance

-106 µm/+31 µm
  • Atomized, CoCrAlY alloy
CO-110-1 (128 KB)